Reduction of ferrite phase in austenitic stainless steels by controlling content of Cr-Ni equivalent
AISI 316L austenitic stainless steels are very common in the industry. Large amounts of this material are discarded as a chisel and can subsequently be used as recycled material for casting. In marine environments (highly corrosive), this type of steel presents intragranular corrosion, specifically...